Parallel abstracts


This study is to investigate the physical proper properties of an injectable form calcium sulfate and to evaluate its osteoconductive ability in a rabbit model. The particle size was 2200±90 nm. The setting time of liquid calcium sulfate was 17.0±0.5 min. The mean compressive and bending strengths were 44.9±9.59 and 14.06±2.06 Mpa, respectively. In rabbits, a liquid calcium sulfate was injected into a 5 x 10 mm cylindrical hole at the medial femoral condyle. Complete resorption of the injectable calcium sulfate occurred by 8weeks with a ring of remodeling cancellous bone formed in the peripheral region. By 12 weeks, the calcium sulfate in the bone defect was completely absorbed and replaced by regenerated trabecular bone.

Parallel keywords

calcuium sulfate bone substitute osteoconducton